Synthetic Underlayment

Also known as synthetic roofing underlayment · synthetic felt · polypropylene underlayment · woven underlayment · non-bitumen synthetic underlayment · UDL

Synthetic underlayment is a lightweight, tear-resistant sheet of woven or laminated polypropylene or polyethylene that is mechanically fastened over the roof deck as an alternative to asphalt-saturated felt.

5 min read6 sourcesNorth America
Cite this entry"Synthetic Underlayment." roof.wiki. https://roof.wiki/synthetic-underlayment/ (accessed 2026-11-03).
Materials
Polypropylene or polyethylene, woven, spun-bonded or laminated
Typical roll
About 4 x 250 ft (1.2 x 76 m)
Typical permeance
Below 1 perm for most; permeable types 10 perms or more
UV exposure
Typically 4-12 months, varies by product
Fasteners
Cap nails or cap staples
Standards
ASTM D8257; previously ICC-ES AC188 / AC207 evaluations
Code recognition
D8257 expected in the 2024 IBC and IRC

Quick answers

What is Synthetic Underlayment?
Synthetic underlayment is a lightweight, tear-resistant sheet of woven or laminated polypropylene or polyethylene that is mechanically fastened over the roof deck as an alternative to asphalt-saturated felt.
Which standards apply to Synthetic Underlayment?
ASTM D8257; previously ICC-ES AC188 / AC207 evaluations

Synthetic underlayment is a roofing underlayment made of polymer sheet — usually polypropylene or polyethylene, woven, spun-bonded or laminated, often with a polymer coating and a slip-resistant face — that is rolled out over the roof deck and fastened with cap nails or cap staples before the roof covering is installed.12 It does the same job as traditional roofing felt: it sheds water that gets past the shingles, tiles or metal, keeps the deck dry during construction, and separates the covering from the deck. It is distinct from self-adhered membranes such as ice and water shield and high-temperature underlayment, which bond to the deck, and is often used together with them, the self-adhered sheet at eaves and valleys and the synthetic over the rest of the roof.

Structural deckVapour control layerInsulationCover boardWaterproof membrane Hot-air welding fuses overlapping sheets into one continuous skin
Inside a flat roof

Synthetics have been on the market for more than 20 years and grew in market presence for years before a consensus standard for them existed.34 On roof.wiki the parent topic is roofing underlayment.

How it differs from felt

Asphalt felt has a core of organic paper (or, in some products, inorganic fibres) saturated with asphalt. That core absorbs moisture, which can make felt wrinkle and cause waviness under shingles, and it tears easily, especially around fasteners and under foot traffic or high wind.23 Synthetics were developed to give much higher tensile and tear strength.3 In practice they differ from felt in several ways:12

  • Weight and coverage — rolls are typically about 4 ft (1.2 m) wide and up to 250 ft (76 m) long, against 3 ft (0.9 m) by 72-144 ft (22-44 m) for felt, giving more coverage per unit weight and fewer rolls to carry onto the roof.
  • Tear resistance — high, so the sheet survives wind and foot traffic while the roof is dried in.
  • Exposure — most can be left uncovered for about 4-12 months, and a few for longer; one product was approved for 30 months. Felt is meant to be covered quickly.
  • Cold-weather handling — synthetics stay pliable in cold, whereas felt can crack or split.
  • Traction — varies widely; in published field tests some products had good wet and dry slip resistance, while others became slippery when wet.
  • Cost — about 11-15 US cents per ft2 for vapour-impermeable synthetics and 20-90 cents for vapour-permeable types, against about 5 cents for No. 15 felt and 10 cents for No. 30 (2011 figures).1

Vapour permeance

A key technical difference is breathability. Asphalt felt behaves as a "smart" vapour retarder, at about 5 perms dry and about 60 perms wet, while most synthetic underlayments are below 1 perm and act as vapour barriers.12 Manufacturers therefore recommend ordinary synthetics only over ventilated roof spaces, where the deck can dry downward into a vented attic. Vapour-permeable synthetics of 10 perms or more — one product is rated at 550 perms — are made for unvented assemblies and for roof coverings such as stone-coated steel installed on battens like a ventilated rainscreen, which allow the deck to dry upward.12 Where a vapour barrier at the deck could trap moisture — for example if spray foam may later be applied under the sheathing — some roofing manufacturers recommend felt instead.2 See vapor retarder and vapour-permeable underlay.

Standards and code acceptance

US building codes were written around asphalt felt. The International Building Code, International Residential Code and Florida Building Code referenced the felt standards ASTM D226, D4869 and D6757, which are composition-based; when synthetics were tested to D226, only unrolling, breaking strength and pliability could be checked.34

Manufacturers therefore worked with ICC Evaluation Service to create AC188, Acceptance Criteria for Roof Underlayments, and AC207 for spun-bonded polypropylene underlayments. These are not consensus standards and cannot be referenced in the codes; they are used to obtain ICC-ES evaluation reports as an alternative path to code compliance.34 See ICC-ES evaluation reports.

After about eight years of work by an ASTM task group of contractors, consultants, manufacturers and test laboratories, ASTM published D8257, Standard Specification for Mechanically Attached Polymeric Roof Underlayment Used in Steep Slope Roofing, which adds tests for fastener pull-through, ultraviolet resistance and hydrostatic resistance not found in the felt standards.34 NRCA-sponsored code changes approved by the ICC mean that underlayments meeting D8257 are expected to be recognised in the 2024 IBC and IRC.5

In Florida, synthetics are also approved through state product evaluations, which set fastening schedules and exposure limits for each product.6

Installation

General practice is:1256

  1. Install self-adhered membrane first at eaves, valleys and other areas where codes or climate require an ice barrier; synthetics are not approved as a substitute for peel-and-stick membranes in ice-dam areas.1
  2. Roll out the synthetic horizontally from the eaves, with the printed side up and laps shingled with the flow of water; printed lap lines and nail patterns guide placement.
  3. Lap at least as the manufacturer specifies — about 50% (half-lap) is required on low slopes down to 3:12, where two layers of felt would traditionally be used.2
  4. Fasten with cap nails or cap staples — standard staples and plain roofing nails can tear or puncture the sheet and allow capillary leaks.1 A Florida evaluation for one product, for example, calls for fasteners at 9 in (229 mm) centres on all laps and 12 in (305 mm) centres in two staggered rows in the field.6 In US high-wind areas the codes set the cap size, shank diameter and spacing (see cap nails).5
  5. Seal laps or penetrations with tape or sealant where the manufacturer recommends, since laps can wick water.1
  6. Cover within the exposure limit stated by the manufacturer — 30 to 180 days for the products in one Florida evaluation.6

Performance and failure modes

Synthetics resist tearing and wind far better than felt during construction, and do not wrinkle when wet.23 Problems include:

  • UV degradation when left exposed beyond the rated period;1 see UV degradation;
  • slips and falls on products with poor wet traction, or on dusty or frosty sheets;1
  • condensation on the underside of low-perm synthetics over poorly ventilated or unvented roofs;12
  • blow-off or tearing where too few or the wrong fasteners were used;
  • lap wicking where laps were too narrow or unsealed;1
  • warranty problems when products are installed contrary to the manufacturer's requirements.1

Where synthetic underlayment is used

Synthetic underlayment is widely used beneath asphalt shingles, metal and tile on new and replacement roofs in North America, alongside felt, which remains in use where its vapour permeance or low cost is preferred.123

Eave · starter course first Courses go on fromthe eave up. Each onecovers the nails below;joints are offset.
How shingles are laid

Sources

Reviewed 2 November 2026 · 6 sources · 6 cited inline · Editorial policy · Plain-text version · Suggest a correction

  1. Synthetic Roofing UnderlaymentsFine Homebuilding · finehomebuilding.com
  2. Understanding Roof UnderlaymentsDECRA Roofing Systems · decra.com
  3. High-tech protectionProfessional Roofing (NRCA) · professionalroofing.net
  4. New ASTM Standard Replaces Felt Standards for Qualification of Synthetic UnderlaymentsFlorida Roofing and Sheet Metal Contractors Association · floridaroof.com
  5. Understanding underlaymentProfessional Roofing (NRCA) · professionalroofing.net
  6. Evaluation Report FL16884-R4: TARCO synthetic underlaymentsFlorida Building Commission · floridabuilding.org

From the community

Know this topic first-hand? Share a photo you took, a correction with a source, or local knowledge. Every contribution is reviewed before it appears.

Contribute to Synthetic Underlayment

Loading…