Synthetic and Composite Roofing

Also known as composite roofing · synthetic roofing · polymer roofing · plastic roof tiles · composite shingles · synthetic roof shingles

Moulded roof coverings made from virgin or recycled polymers, rubber and mineral fillers that imitate natural slate, wood shakes, clay tile and thatch at a fraction of their weight.

5 min read7 sourcesNorth AmericaEuropeGlobal
Cite this entry"Synthetic and Composite Roofing." roof.wiki. https://roof.wiki/synthetic-roofing/ (accessed 2026-11-03).
Main materials
Virgin and recycled polyolefins, recycled plastic, rubber, mineral fillers
Imitates
Slate, cedar shake, clay barrel tile, asphalt shingle, thatch
North American evaluation
ICC-ES AC07 special roofing systems
Fire
Class A usually only over a specified fire-rated underlayment
Impact
UL 2218 / FM 4473 Class 4 common
Typical minimum slope
3:12 (25%)
Weight
About 250-310 lb per 100 sq ft (12-15 kg/m²)

Synthetic (composite) slates

Layers from the surface down.

  1. Deck
  2. Underlayment
  3. Composite slates
  • Moulded polymer or rubber units shaped and textured like slate.
  • Thicker at the butt than natural slate (often ½ in), tapering toward the head.
  • Laid from the eave up; each course laps down over the one below.

Model shows typical proportions, not a specification. Follow the manufacturer's instructions and local code.

Types of Synthetic and composite roofing

Quick answers

What is Synthetic and Composite Roofing?
Moulded roof coverings made from virgin or recycled polymers, rubber and mineral fillers that imitate natural slate, wood shakes, clay tile and thatch at a fraction of their weight.
How much does Synthetic and Composite Roofing weigh?
About 250-310 lb per 100 sq ft (12-15 kg/m²)

Synthetic or composite roofing is a broad class of steep-slope roof coverings made mainly from plastics and rubber, usually with mineral fillers, pigments and stabilisers, and moulded or injection-formed to imitate a traditional material. The best-known products copy natural slate and split cedar shakes, but there are also synthetic Spanish barrel tiles, asphalt-style "architectural" shingles, and imitation palm and reed thatch.1234 The category is defined by what the products are made of rather than by their shape: one manufacturer may make slate, shake and tile profiles from the same compound, installed in much the same way.

Courses go on from theeave up. Each is held by asway the next course covers.
How thatch is laid

On roof.wiki the umbrella topic links three more specific articles, synthetic slate, synthetic shake and the synthetic roof tile, together with synthetic thatch and rubber shingles. Products made of fibre cement, bitumen or metal that also imitate slate or tile are usually treated separately, as fibre-cement slates, asphalt shingles and stone-coated or pressed metal tiles.

Materials

Most synthetic roofing falls into a few material groups:

  • Polyolefins and engineered polymers. Blends of virgin and recycled polyolefin polymers (polyethylene and polypropylene families) are the basis of many injection-moulded slates and shakes.1 Other makers describe their compound only as a polymeric roof covering or a molded synthetic polymer blend.23
  • Recycled plastic composites. Compression-moulded products may contain up to 85 percent recycled plastic, with mineral pigments, ultraviolet stabilisers and impact modifiers.4 A British lightweight interlocking tile is made with 75 percent recycled content.5
  • Rubber and rubber-plastic blends. Recycled tyre rubber, often blended with plastics, is used in some slate- and shake-style products and in rubber shingles.
  • Mineral-filled composites. Earlier artificial slates were made from mineral fibres bound in cement or resin; heritage bodies note that such products tend to look rigid and manufactured and can fade.6

All polymer roofing must resist ultraviolet light, which embrittles and discolours plastics. Manufacturers add UV stabilisers and test weathering by accelerated exposure: one tile specification, for example, limits tensile-strength loss to 10 percent after 2,500 to 4,500 hours of xenon-arc exposure under ASTM G155, and colour change to no more than 4 Hunter units after 2,500 hours.4

How the products are evaluated

Because synthetic roofing is not covered by a traditional product standard in the way that asphalt shingles, clay tiles or slate are, North American products are usually approved through evaluation reports against ICC-ES acceptance criteria AC07 for special roofing systems, which then allow them under the International Building Code and International Residential Code.13 Typical evaluations combine several tests:

head lap Rafter + battens Slates hang in courses from the eave up.Each is nailed (or hooked) to a batten andreaches two courses up, so there are alwaysat least two thicknesses over the roof.
How slates are fixed
  • Fire: ASTM E108 / UL 790. Many products reach Class A only over a specified fire-resistant underlayment or barrier board, and fall back to Class C over ordinary felt; one polyolefin product is Class A over a gypsum-based barrier board and Class C when a single ply of No. 30 felt is substituted.1 Another range is listed Class A in several assemblies and Class C in one.2
  • Impact: UL 2218 and FM 4473; Class 4, the highest rating, is common.234
  • Wind: uplift under UL 580 and UL 1897 or, for shingle-format products, ASTM D3161 Class F and ASTM D7158 Class H; Florida products are also tested under TAS 100, TAS 107 and TAS 125, including High-Velocity Hurricane Zone provisions.134
  • Durability: freeze-thaw cycling (for example from -40 °F to 180 °F, -40 °C to 82 °C, with no crazing or cracking) and accelerated weathering.4

In Britain, comparable products are assessed by BBA certificates and fixed to BS 5534.5

Installation

Synthetic slate, shake and tile are installed much like the materials they imitate, but each product has its own rules, which are written into the evaluation report:

  • Deck: solid sheathing, typically at least 15/32 in (12 mm) plywood or 7/16 in (11 mm) OSB.31
  • Slope: minimums of 3:12 (25 percent) are typical; at least one tile maker requires 4:12 for warranty coverage and an ice-dam membrane over the whole roof between 3:12 and 4:12.134 Exposures are often reduced on lower slopes; one slate product lays at 6 in (152 mm) exposure on 3:12 roofs and 7 in (178 mm) above 6:12.1 The British lightweight tile is rated down to 12.5 degrees.5
  • Underlayment: No. 30 felt to ASTM D226 Type II or a synthetic underlayment, an ice barrier at eaves in cold climates, and a fire-rated underlayment where Class A is needed.134
  • Fasteners: corrosion-resistant ring-shank nails or screws, often several per piece, driven flush; one asphalt-style product calls for at least six nails per shingle, and a tile product for two ring-shank nails per piece, with stainless steel recommended near the coast.34
  • Spacing: synthetic slates are often laid with small gaps (for example 3/8 in, 10 mm) between pieces to allow for thermal expansion of the polymer.1

Weight

Low weight is the main technical advantage. A composite barrel tile is specified at a maximum of 300 lb per 100 sq ft (about 15 kg/m²), and composite shakes and slates at about 300 to 310 lb per 100 sq ft.4 One maker quotes 252 lb per square for its composite Spanish tile and contrasts it with clay tile, which often needs extra structure.7 The British plastic tile weighs under 8 kg/m² (about 1.6 lb/sq ft), roughly 80 percent less than concrete tiles.5 By comparison, natural slate and clay or concrete tile commonly weigh several times as much, which is why synthetic products are used where a heavy roof would need structural reinforcement.

Durability and lifespan

Manufacturers commonly offer long limited material warranties, often 40 to 50 years, with shorter colour warranties.45 The products are young compared with what they imitate, however, and their long-term field record is limited. Heritage authorities point out that natural slate roofs can last 60 to 125 years or more, that several artificial roofs may be installed in the life of one slate roof, and that the total initial cost of an artificial roof is often only marginally less once labour, flashing and tear-off are counted.6 The US National Park Service does not recommend artificial slate for restoration work because of its manufactured appearance and the risk of fading.6

Typical concerns with synthetic roofing are colour fade and gloss change from UV exposure, warping or buckling if expansion gaps are omitted, brittleness in cold weather, and the fire rating depending on the underlayment actually installed.

Uses

Synthetic roofing is used on houses where owners want the look of slate or shake without the weight, cost or maintenance; in hail-prone regions where Class 4 impact ratings may qualify for insurance discounts; on light timber-framed and modular buildings, garden buildings and extensions; and in resorts and theme parks for imitation thatch.52 On listed or historic buildings, conservation bodies generally prefer repair with natural materials.6

Sources

Reviewed 2 November 2026 · 7 sources · 7 cited inline · Editorial policy · Plain-text version · Suggest a correction

  1. Code Compliance Research Report CCRR-0283: REVIA Synthetic Roofing ShinglesIntertek / Florida Building Commission · floridabuilding.org
  2. Synthetic Roof Tiles Specification 07 31 00ARCAT (Brava Roof Tile) · arcat.com
  3. Envirotile: the lightweight sustainable roof tileBarbour Product Search · barbourproductsearch.info
  4. Should I replace my slate roof with a synthetic?US National Park Service · nps.gov
  5. Clay Roof Tile vs Brava Composite Spanish TileBrava Roof Tile · bravarooftile.com

From the community

Know this topic first-hand? Share a photo you took, a correction with a source, or local knowledge. Every contribution is reviewed before it appears.

Contribute to Synthetic and Composite Roofing

Loading…