Hip and Ridge Shingles

Also known as ridge cap shingles · hip and ridge caps · cap shingles · ridge shingles · high-profile ridge cap

Narrow asphalt capping shingles, either factory-made accessories or pieces cut from three-tab shingles, that are bent over the hips and ridge of a shingle roof to seal the joint where two slopes meet.

5 min read6 sourcesNorth America
Cite this entry"Hip and Ridge Shingles." roof.wiki. https://roof.wiki/hip-and-ridge-shingles/ (accessed 2026-11-03).
Typical piece size
About 12 × 12–13¼ in (305 × 305–337 mm), split from 36 in (914 mm) strips
Typical exposure
5⅝ in (143 mm) standard; up to 8 in (203 mm) high-profile
Fasteners
Two corrosion-resistant roofing nails per piece, covered by the next piece
Lay direction
Start at the end opposite the prevailing wind
Product standards
ASTM D3462 (US), CSA A123.5 (Canada)
Wind classes
ASTM D3161 Class F and ASTM D7158 Class H on some products
Laminated shingles
Not suitable for cutting into caps

Hip and ridge shingles, also called cap shingles or ridge caps, are the small units that cover the joints along the hips and ridge of an asphalt shingle roof. Each piece is bent across the line where two slopes meet and lapped over the one before it, much like a run of overlapping saddles. Before factory-made accessories were widely available, roofers made them by cutting standard three-tab shingles into thirds; today most manufacturers sell purpose-made, often thicker capping shingles in colours matched to their field shingles.45

On tile and slate roofs the same job is done by ridge and hip tiles or metal rolls (see ridge and hip tiles and ridge cap installation). This article covers the asphalt products only.

head lap Rafter + battens Slates hang in courses from the eave up.Each is nailed (or hooked) to a batten andreaches two courses up, so there are alwaysat least two thicknesses over the roof.
How slates are fixed

Types

Cut three-tab caps

The traditional method is to cut a self-sealing three-tab shingle across at its tab slots into three pieces of about 12 in (305 mm) each, trim the top corners to a taper so the lapped part does not show, and bend each piece over the ridge. The result is thin and flat. Some manufacturers still allow it under limits: one permits its three-tab shingle to be cut vertically into thirds for hips and ridges only when that same shingle is used on the main roof.5 Cut caps are usually 20- or 25-year products, so on a roof of longer-rated laminated shingles they can become the weak point.4

Laminated ("architectural") shingles cannot be used this way. Their two bonded layers and different sealant strip placement mean the cut pieces do not bend or seal like three-tab, and one manufacturer states that using them for caps voids the warranty.5 See architectural shingle.

Eave · starter course first Courses go on fromthe eave up. Each onecovers the nails below;joints are offset.
How shingles are laid

Pre-cut (perforated) caps

Most purpose-made caps come as strips that the roofer splits into pieces at perforations or score lines, usually into three 12 in (305 mm) pieces from a 36 in (914 mm) strip.13 They are often pre-tapered: one product has a 1 in (25 mm) factory taper on the top of each side of each piece.2 Some have a factory sealant strip or dots set to bond each piece to the one below.24 Pieces are made to be bent, but they bend more easily and crack less when warm.12

High-profile and laminated caps

High-profile caps are thicker, sometimes made of two or more layers or with a moulded shape, so the ridge line looks heavier and suits the shadow lines of laminated field shingles. They are colour-blended to match particular shingle ranges.4 One high-profile type comes as 12 × 12 in (305 × 305 mm) pieces, scored three to a 36 in strip, laid at an 8 in (203 mm) exposure.1

Polymer-modified and impact-rated caps

Some caps are made with polymer-modified asphalt to improve flexibility and impact resistance, so that impact-rated roofs can have matching ridges. One such product meets ASTM D3462 and CSA A123.5 as its product standards, is rated Class F under ASTM D3161 and Class H under ASTM D7158 for wind, and Class 4 for impact under FM 4473.3 See polymer-modified (SBS) shingles.

Dimensions and coverage

Products vary, but common figures are:

  • Piece size: about 12 in (305 mm) along the ridge by 12 to 13¼ in (305–337 mm) across it.13
  • Exposure: about 5⅝ in (143 mm) for standard-thickness caps and up to 8 in (203 mm) for some high-profile caps; using a larger exposure than specified gives less coverage per bundle.123
  • Coverage: one standard-profile product yields 78 pieces per bundle, covering about 36.5 linear ft (11.1 m) of hip or ridge.3

Installation

Instructions differ by product, so the manufacturer's sheet governs. The common steps are:

  1. Starter. The first piece at the bottom of a hip or at the start of a ridge is often doubled. One manufacturer has a 12 in piece cut along its headlap line to give a double-thick starter about 4 × 11½ in (102 × 292 mm).1
  2. Direction. On a gable roof, the ridge is started at the end facing away from the prevailing wind, so the laps face downwind.12 On hip roofs, the hips are capped first from eave to ridge. Then the ridge is capped from each end, meeting in the middle.2
  3. Bending. Each piece is bent evenly over the ridge or hip and centred on it. In cold weather, shingles are warmed first, by keeping them in a heated area or laying them in the sun.12
  4. Nailing. Two nails per piece, one on each side, about 1 in (25 mm) in from the edge and covered by the next piece. One product sets them 6¼ in (159 mm) above the butt, below the factory sealant.2 Instructions call for corrosion-resistant 10- to 12-gauge roofing nails with heads of at least ⅜ in (9.5 mm), driven flush. They should go at least ¾ in (19 mm) into board decks or just through plywood and OSB, and one maker sets a minimum nail length of 1½ in (37 mm).12 Overdriven nails damage the shingle, and raised nails reduce wind resistance.1
  5. Finishing. The exposed nails of the last piece are covered with roofing cement.2

Where self-sealing is delayed by cold weather, small dabs of asphalt plastic cement (ASTM D4586) can be placed between pieces, though too much can cause blistering.1 For high-wind areas, one manufacturer calls for a ¼ in (6 mm) bead of polyurethane sealant (ASTM C920) on each side of each headlap.1

Over ridge vents

Where a ridge vent is fitted, the deck is cut back along the peak, the vent is fixed over the slot, and the cap shingles are nailed through the vent into the deck. One vent maker calls for a slot cut no more than ¾ in (19 mm) either side of the peak, and for 2½ in (64 mm) nails through the cap shingles so that they penetrate ¾ in into the deck, or right through it.6 Thicker caps over a vent need longer nails still, and caps must be checked against the vent maker's instructions.

Performance and failure modes

Hips and ridges get the highest wind suction on a pitched roof, and the cap pieces stand above the plane of the roof, so their seal and nailing matter more than in the field (see roof wind pressure zones). Factory adhesive strips on purpose-made caps are designed to cut wind-related callbacks.4 Typical failures are:

  • Cracking across the bend, especially when shingles are bent cold or are brittle with age.12
  • Blow-off of pieces that never sealed, or that were nailed too high or too low.1
  • Nail pops and leaks where nails are short over ridge vents or are left exposed.26
  • Granule loss and ageing ahead of the field, since caps face the weather on both sides.

Replacing worn caps is a common repair, and it is easier when the cap matches the field shingle range.

Use and history

Capping with shingles cut from the field shingle followed the spread of strip shingles in North America in the 20th century (see history of asphalt shingles). Because laminated shingles cannot be cut into caps, their spread pushed roofers towards dedicated accessories.5 Manufacturers now give the caps warranty terms tied to their laminated ranges, while cut three-tab caps normally carry 20- or 25-year terms.4 Dedicated caps are used on most new asphalt shingle roofs in the United States and Canada, while cut three-tab caps survive mainly on three-tab roofs.5

Sources

Reviewed 2 November 2026 · 6 sources · 6 cited inline · Editorial policy · Plain-text version · Suggest a correction

From the community

Know this topic first-hand? Share a photo you took, a correction with a source, or local knowledge. Every contribution is reviewed before it appears.

Contribute to Hip and Ridge Shingles