Galvanic Corrosion and Metal Compatibility

Also known as bimetallic corrosion · dissimilar metal corrosion · galvanic series · metal compatibility

Galvanic corrosion is accelerated attack on one metal when it touches, or is wetted by run-off from, a more noble metal; it governs which roof metals can be combined.

1 min read5 sourcesGlobal
Cite this entry"Galvanic Corrosion and Metal Compatibility." roof.wiki. https://roof.wiki/galvanic-corrosion/ (accessed 2026-11-02).
Needed for corrosion
Two metals, electrical contact, electrolyte
Outdoor risk threshold
Anodic index difference above ~0.15 V
Classic bad pairing
Copper with aluminium, zinc or galvanized steel

When two different metals are in electrical contact and wetted by an electrolyte such as rain, dew or salty air, they form a small battery. The more active metal (the anode) corrodes faster than it would alone, while the more noble metal (the cathode) is protected. On roofs this explains why some flashings, fasteners and gutters fail early when mixed with the wrong metal.

The galvanic series

Engineers rank metals by an "anodic index". From more noble to more active, approximate values are:

  • Copper about -0.35 V
  • Stainless steel (18% chromium) about -0.50 V
  • Tin and tin-lead solder about -0.65 V
  • Lead about -0.70 V
  • Carbon steel about -0.85 V
  • Wrought aluminium about -0.90 V
  • Galvanized steel about -1.20 V
  • Zinc about -1.25 V

Outdoors, a difference of more than about 0.15 V is considered risky. Copper with aluminium, zinc or galvanized steel is a classic bad pairing.

Area and flow

A small anode attached to a large cathode corrodes fastest, so a steel screw in copper sheet fails quickly, while a copper rivet in steel is less severe. Water flowing from a noble metal onto an active one carries dissolved ions that also cause attack: copper run-off onto Galvalume, zinc or aluminium gutters is a common problem.

Practical rules

  • Use fasteners of the same metal or a compatible, more noble one: copper, bronze or 300-series stainless steel with copper; stainless or aluminium fasteners with aluminium, never bare or ordinary steel.
  • Separate dissimilar metals with bituminous coatings, membranes or non-conductive spacers.
  • Keep copper and its run-off away from aluminium, zinc, galvanized steel and aluminium-zinc coated steel.

Famous example

The Statue of Liberty suffered galvanic attack where its copper skin met its wrought iron framework after the original shellac insulation failed; restoration replaced the insulation with PTFE.

Sources

  1. Galvanic corrosionWikipedia · en.wikipedia.org
  2. 14.3. Copper Roofing (architectural specifications)Copper Development Association · archive.copper.org
  3. Aluminum Roofing Fasteners: Concealed vs Exposed ExplainedInterlock Roofing · interlockroofing.com
  4. Metal Roofing Problems: The Honest 20-Year GuideInterlock Roofing · interlockroofing.com
  5. Durability: Compatibility (NZ Metal Roof and Wall Cladding Code of Practice)NZ Metal Roofing Manufacturers · metalroofing.org.nz