# Asphalt and Aluminium Roof Coatings

> Asphalt roof coatings are bitumen-based liquids (water emulsions or solvent cutbacks, often fibred) brushed or sprayed onto bituminous and metal roofs; aluminium-pigmented versions add a reflective metallic finish.

- URL: https://roof.wiki/asphalt-roof-coating/
- Topic: Low-Slope & Flat Roof Systems
- Also known as: asphalt emulsion; emulsified asphalt coating; cutback coating; fibered aluminum roof coating; aluminum roof coating; aluminium bitumen paint; bitumen roof paint; silver roof coating
- Regions: North America, Europe
- First published: 2026-11-02 · Last reviewed: 2026-11-02
- Cite as: "Asphalt and Aluminium Roof Coatings." roof.wiki. https://roof.wiki/asphalt-roof-coating/

## Key facts

- **Emulsion standard:** ASTM D1227 (Types I-III; Class 1 clay, Class 2 chemical emulsifier)
- **Solvent-borne standard:** ASTM D4479 (asbestos-free asphalt roof coatings)
- **Aluminium coating standard:** ASTM D2824 (Type I non-fibred, Type III non-asbestos fibred)
- **Fibred emulsion coverage:** 3-4 US gal per 100 ft2 (about 1.2-1.6 L/m2); 5-6 gal for gravel
- **Aluminium coverage:** 1-1.5 US gal per 100 ft2 (about 0.4-0.6 L/m2)
- **Aluminium coating reflectance (example):** 0.63 initial / 0.55 aged; emittance 0.46-0.53; SRI 62/52
- **Minimum slope (D1227):** 4% (1/2 in per ft)

**Asphalt roof coatings** are liquid products made from asphalt (bitumen) that are applied cold to the surface of an existing roof to protect it from sunlight and weather, to renew a weathered surface, or to embed reinforcing fabric and gravel. They fall into two chemical families — **emulsions**, in which asphalt is dispersed in water, and **solvent-borne** or "cutback" coatings, in which asphalt is thinned with petroleum solvents — and either kind may be **fibred** for body and crack-bridging.[1][2] **Aluminium roof coatings** are asphalt coatings pigmented with flakes of aluminium, which leaf to the surface as the film dries and give a bright, reflective silver finish.[3]

Under the wider topic of [roof coatings](https://roof.wiki/roof-coating/), these bitumen-based products are distinct from the elastomeric families — [acrylic](https://roof.wiki/acrylic-roof-coating/), [silicone](https://roof.wiki/silicone-roof-coating/) and polyurethane — which are based on synthetic polymers, are usually white, and are designed to form a continuous rubbery film. Asphalt and aluminium coatings are older, cheaper and chemically compatible with [built-up](https://roof.wiki/built-up-roofing/) and [modified-bitumen](https://roof.wiki/modified-bitumen-roofing/) roofs, but they are generally less elastic and, apart from aluminium, absorb rather than reflect sunlight.

## Types and standards

In North America the main products are classified by ASTM specifications:

- **ASTM D1227 — emulsified asphalt protective coatings.** Type I and Type II contain fillers or fibres (Type I historically included asbestos; Type II uses other fibres), while Type III has no fibrous reinforcement. Each type is split into Class 1, emulsified with mineral colloids such as clay, and Class 2, emulsified chemically. The specification covers coatings for built-up roofs and other exposed surfaces with a slope of at least 4% (1/2 in per ft, 42 mm/m).[1]
- **ASTM D4479 — asbestos-free asphalt roof coatings.** These are solvent-based: an asphalt base, volatile petroleum solvents and mineral stabilisers, mixed for brushing or spraying. Type I uses self-healing, adhesive, ductile asphalts; Type II uses high-softening-point, lower-ductility asphalts.[2]
- **ASTM D2824 — aluminium-pigmented asphalt roof coatings.** Type I is non-fibred, Type II was fibred with asbestos, and Type III is fibred with non-asbestos material. The specification controls water, non-volatile and metallic aluminium content and includes a luminous reflectance requirement; the coatings are intended for roofing or masonry surfaces by brush or spray.[3]

A typical fibred emulsion sold to D1227 Type II Class I is a blend of asphalt, bentonite clay, inorganic fibres and water, with about 44-51% asphalt and a calculated VOC of zero.[4] Typical fibred aluminium coatings to D2824 Type III combine asphalt, aluminium flake, solvents and reinforcing fibres; one contains at least 14% metallic aluminium by weight and 57% non-volatile matter, with a VOC limit of 400 g/L,[5] and another lists a maximum VOC of 450 g/L.[6] Because solvent-borne coatings contain volatile organic compounds, they are subject to regional air-quality limits that vary by jurisdiction.

## Uses

Asphalt and aluminium coatings serve several distinct roles:

- **Maintenance surfacing** of smooth-surfaced BUR and mod-bit roofs whose asphalt has dried and crazed, typically at 3-4 US gal per 100 ft2 (about 1.2-1.6 L/m2) for a fibred emulsion.[4]
- **Embedment coat** for polyester or glass reinforcing fabric in cold-process repairs and [cold-applied roofing](https://roof.wiki/cold-applied-roofing/), also at about 3-4 gal per 100 ft2.[4]
- **Gravel surfacing** — a heavier coat of about 5-6 gal per 100 ft2 (2.0-2.4 L/m2) into which gravel is broadcast.[4]
- **Base coat for aluminium** — the aluminium coating is laid over a cured emulsion or directly over sound bitumen.[4][6]
- **Protective finish on metal** — aluminium coatings are applied to corrugated metal and tin roofs as well as to BUR, SBS and APP surfaces.[5]

Aluminium coatings are generally not intended for single-ply membranes; one manufacturer restricts its product to multi-ply bituminous systems.[5]

## Reflectance of aluminium coatings

The aluminium flakes give these coatings a much higher solar reflectance than black asphalt, but the metallic surface also has a low **thermal emittance**, meaning it sheds absorbed heat poorly by radiation. For one fibred aluminium coating rated under the [Cool Roof Rating Council](https://roof.wiki/cool-roof-rating-council/) programme, published values are a solar reflectance of 0.63 initially and 0.55 after three years, with a thermal emittance of 0.46 rising to 0.53, giving a [solar reflectance index](https://roof.wiki/solar-reflectance-index/) of 62 initial and 52 aged.[6] Another product lists a reflectance of 62%.[5] The low emittance pulls the SRI down, so aluminium coatings can fall short of [cool roof](https://roof.wiki/cool-roof/) requirements that set a minimum emittance or SRI, even though their reflectance is moderate (see [thermal emittance](https://roof.wiki/thermal-emittance/)). Aluminium surfaces also dull as they weather and collect dirt.

## Application

A typical cold-applied sequence is:[4][6]

1. **Inspect and repair** — re-adhere loose laps, cut and patch blisters, and seal open seams with fabric and roof cement, allowing the cement to cure (one manufacturer asks for 30 days before coating).
2. **Clean** the roof of dirt, loose granules and debris and make sure no water is standing; scrub areas where water has ponded.
3. **Prime** badly weathered or alligatored asphalt with an emulsion primer or a fibred emulsion.
4. **Apply the asphalt coat** by brush, squeegee, roller or spray at the stated rate, allowing it to dry completely between coats — from 6-24 hours in hot dry weather to 2-7 days in cool damp weather for one emulsion.[4]
5. **Apply the aluminium top coat** once the emulsion has cured, usually 3-5 days later, at about 1-1.5 gal per 100 ft2 (0.4-0.6 L/m2, roughly 16-24 wet mils). Aluminium coatings are not thinned, and over-brushing disturbs the leafing of the flakes.[5][6]

Weather limits matter. Emulsions must not freeze in storage or before they dry, and are not applied below about 10 C (50 F) or when rain is expected within 24 hours.[4] Solvent aluminium coatings are applied at roughly 4-49 C (40-120 F) and need to be kept dry for 24-48 hours; new asphalt roofs should weather for at least 90 days before an aluminium coat is applied, or the oils in fresh asphalt bleed through and discolour it.[5][6]

## Performance, limits and failure modes

Asphalt coatings are a maintenance layer rather than a new waterproofing system. Their main limits are:

- **Ponding water** — asphalt coatings form water-soluble products as they weather; on roofs pitched under 1/2 in per ft (4%) these collect in low spots, and long-standing water causes abnormally rapid deterioration.[4] Cold-process coatings are recommended only where the deck has positive drainage, which the NRCA defines as no standing water 48 hours after rain stops (see [positive drainage](https://roof.wiki/positive-drainage/)).[6]
- **Cracking and alligatoring** as the asphalt oxidises in sunlight, especially for unpigmented black coats; aluminium pigment slows this by blocking UV.
- **Bleed-through and discolouration** when an aluminium coat is applied over fresh asphalt or uncured flashing cement.[6]
- **Incompatibility** with single-ply membranes such as EPDM, TPO and PVC.[5]

Some emulsions and aluminium coatings carry UL Class A or B listings when applied as part of a tested roof assembly.[4][6] Fire, wind and approval listings depend on the full system, so specifiers consult FM RoofNav or UL directories for application rates.[5]

## Where they are used

Asphalt emulsions and fibred aluminium coatings have long been the standard maintenance products for bituminous low-slope roofs on commercial, agricultural and residential buildings in North America, and for coating corrugated metal roofs on barns, sheds and manufactured homes.[5][6] On larger commercial roofs, many owners now choose white elastomeric coatings or new reflective cap sheets where energy codes require higher reflectance (see [cap sheet](https://roof.wiki/cap-sheet/)).

## Sources

1. ASTM D1227/D1227M-13(2024) Standard Specification for Emulsified Asphalt Used as a Protective Coating for Roofing — ASTM International. https://store.astm.org/d1227_d1227m-13r24.html
2. ASTM D4479/D4479M-07(2024) Standard Specification for Asphalt Roof Coatings - Asbestos-Free — Technicke normy (ASTM listing). https://www.technickenormy.cz/astm-d4479-d4479m-07r24-standard-specification-for-asphalt-roof-coatings-asbestos-free
3. ASTM D2824/D2824M-18 Standard Specification for Aluminum-Pigmented Asphalt Roof Coatings, Nonfibered, and Fibered without Asbestos — ASTM International. https://store.astm.org/d2824_d2824m-18.html
4. HE307 Fibered Asphalt Emulsion product data — Henry Company via BuildSite. https://www.buildsite.com/pdf/henry/HE307-Fibered-Asphalt-Emulsion-Product-Data-2142484.pdf
5. Fibrated Aluminum Roof Coating data sheet (RS-2067) — Johns Manville. https://JM.COM/content/dam/jm/global/en/commercial-roofing/Data%20sheets/Cements%20and%20Coatings%20Data%20Sheets/RS-2067_FibratedAluminumRoofCoating.pdf
6. 98 Fibered Aluminum Roof Coating product data — Karnak via BuildSite. https://www.buildsite.com/pdf/karnak/98-Fibered-Aluminum-Roof-Coating-Product-Data-1804959.pdf